8at% Ni at room temperature is composed of columnar B2 and granular metastable phase;the metastable phase is a disordered Al made up of Ti and Ni atoms;there is a vacancy short-range order in RS TiNi ribbon and a vacancy long-range order in RS TiNi ribbon followed by aging.
快速凝固后室温下合金的组织由柱状B2相和粒状亚稳相构成;亚稳相是由Ti、Ni两元素原子构成的无序面心立方结构;快速凝固后合金中的空位呈短程有序分布,而在450℃5min时效后呈长程有序分布,在电子衍射图上形成1/2100和1/4210额外斑点。
Experimental results show that short range atomic disordering takes place during ageing in the martensite state whereas the long range order degree remians almost unchanged.
实验结果表明,淬火态CuAlNiMnTi合金在马氏体态时效过程中发生马氏体稳定化现象;在这一过程中DO3长程有序度无明显变化,但发生了原子短程无序。
During parent phase aging, DO_3 atomic reordering occurs, leading to an increase in the degree of long range order.
在马氏体状态时效,DO_3长程有序度无显著变化,没发生类似在母相态的再有序化,主要是原子短程无序化。
The influence of Ni-Al ordering energy from the first to the fourth layer on the atom long range order progress in Ni75Al13Cr12 alloy was investigated by microscopic phase field model.
通过微观相场方法研究了Ni75Al13Cr12合金Ni-Al第一到四层有序能对原子长程有序进程的影响。
Mosaic fragmentation and length range order parameters in FeAl intermetallic compound of type B_2 in the process of ball grinding mills;
球磨中B_2型FeAl的嵌镶碎化和长程有序度
The long range order parameter(LRO) was used to evaluate the degree of ordering of the ordered phase.
25)混合粉末的机械球磨过程,分析球磨1h和5h的粉末在860°C条件下退火4h的物相组成,并采用长程有序参数定量表征了退火得到的有序相的有序程度。