Defect analysis of centrifugal casting brass cage and preventive measures;
离心铸造黄铜的缺陷分析及预防措施
Inhibition Action of the Self-Assembled Monolayers of 3-Amino-1,2,4-triazole on Brass;
3-氨基-1,2,4-三氮唑自组装膜对黄铜的缓蚀作用
Research on Enhancing Dump Leaching of Chalcopyrite by Pyrite;
排土场黄铁矿促进黄铜矿浸出研究
Thiobacillus ferrooxidans bioleaching of chalcopyrite at low temperature;
低温下氧化亚铁硫杆菌浸出黄铜矿
Study of Bacterial Leaching of Chalcopyrite by Strengthening Microwave and Magnetic Field;
微波和磁场强化细菌浸出黄铜矿研究
Corrosion electrochemistry of brass tube in simulated circlating cooling system;
模拟循环冷却系统黄铜管的腐蚀电化学
Analysing the cause of brass tube corrosion in steam turbine condenser;
汽轮机凝汽器黄铜管腐蚀原因分析
Made sample from brass tube fragment,polished the surface of the sample and eroded it with solution of 5% iron trichloride (FeCl3) and 10% hydrochloric acid (HCl),then the photos were taken with Nicon-300 metallographic microscope.
从消除应力腐蚀的环境出发,提出了黄铜管换热器制造过程中对管束进行耐压试验的注意事项。
In order to investigate the size dependence of the plastic deformation properties for metal foil,uniaxial tensile tests of brass foil specimens with different thicknesses and grain sizes are performed at room temperature.
为了研究金属箔的塑性变形性能与尺寸的相关性,在常温下对不同厚度和晶粒尺寸的黄铜箔试样进行了单向拉伸实验。