Defect analysis of centrifugal casting brass cage and preventive measures;
离心铸造黄铜的缺陷分析及预防措施
Inhibition Action of the Self-Assembled Monolayers of 3-Amino-1,2,4-triazole on Brass;
3-氨基-1,2,4-三氮唑自组装膜对黄铜的缓蚀作用
Research on Enhancing Dump Leaching of Chalcopyrite by Pyrite;
排土场黄铁矿促进黄铜矿浸出研究
Thiobacillus ferrooxidans bioleaching of chalcopyrite at low temperature;
低温下氧化亚铁硫杆菌浸出黄铜矿
Study of Bacterial Leaching of Chalcopyrite by Strengthening Microwave and Magnetic Field;
微波和磁场强化细菌浸出黄铜矿研究
Corrosion electrochemistry of brass tube in simulated circlating cooling system;
模拟循环冷却系统黄铜管的腐蚀电化学
Analysing the cause of brass tube corrosion in steam turbine condenser;
汽轮机凝汽器黄铜管腐蚀原因分析
Made sample from brass tube fragment,polished the surface of the sample and eroded it with solution of 5% iron trichloride (FeCl3) and 10% hydrochloric acid (HCl),then the photos were taken with Nicon-300 metallographic microscope.
从消除应力腐蚀的环境出发,提出了黄铜管换热器制造过程中对管束进行耐压试验的注意事项。